Cycoloy树脂CX7720是一种无溴、无氯阻燃PC/ABS树脂,具有高耐热性和薄壁阻燃性能。它是UL-94标准中的1.2 mm v0和1.5 mm 5vb。它的高热变形温度允许该产品被考虑用于需要比传统的fr-pc/abs更高的耐热性的应用。 Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its high heat deflection temperature allows this product to be considered for applications requiring higher heat resistance than conventional FR PC/ABS. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.22 | g/cm³ | ASTM D792 , ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
ASTM D1238 | ||
260℃,2.16kg 260℃,2.16kg |
9.0 | g/10min | ASTM D1238 |
260℃,5.0kg 260℃,5.0kg |
25 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
260℃,5 kg 260℃,5 kg |
22.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
MD:3.2 mm MD:3.2 mm |
0.50 到 0.70 | % | 内部方法 |
吸水率 Water absorption rate |
ISO 62 | ||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
-- -- 3 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield 4 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
断裂 fracture 4 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
屈服 yield 4 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/50 | |
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus |
|||
50 mm跨距 50 mm span 5 |
MPa | ASTM D790 | |
-- -- 6 |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
-- -- 6 , 7 |
MPa | ISO 178 | |
屈服,50 mm跨度 Yield, 50 mm span 5 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 8 |
|||
23℃ 23℃ 8 |
kJ/m² | ISO 179/1eA | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
-30℃ -30℃ 9 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ 9 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ 10 |
kJ/m² | ISO 180-1A | |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,6.4 mm 0.45 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,6.4 mm 1.8 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 11 |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temp |
|||
B50 B50 |
℃ | ASTM D1525 12 , ISO 306/B50 12 | |
B120 B120 |
℃ | ISO 306/B120 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
ASTM E831 , ISO 11359-2 | ||
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831,ISO 11359-2 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831,ISO 11359-2 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
1.00 mm 1.00 mm |
UL 94 | ||
1.20 mm 1.20 mm |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
2.50 mm 2.50 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
3 类型 1, 2.0 in/min |
4 0.051 in/min |
5 0.079 in/min |
6 Yield |
7 80*10*3 sp=62mm |
8 80*10*3 |
9 80*10*4 |
10 80*10*4 mm |
11 标准 B (120°C/h), 载荷2 (50N) |
【新闻资讯】查看全部
化工专业哪家强?国内这几所大学必须上榜!
2021-06-25 搜料网资讯: 有没有童鞋想报化工专业的,快举手! 小编给大家罗列几所国内比较好的化工专业的部分高校~ 首先是两所国内处于金字塔顶端的高校: 1、天津大学 天津大学,简称 天大 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |