公司信息及水印
牌号简介 About |
---|
Lofex A4110聚酯薄膜具有光学透明性,单侧电晕处理,拉伸强度高,延伸率和热收缩率好。该机运行性能优良,使用方便,产品适用于离型膜、复合膜、胶带等。另外,它是一种可以根据客户需求进行厚度控制的产品。 LOFEX ® A4110 Polyester film is optically clear and one side corona treated with excellent properties by tensile strength , proper elongation and the thermal contraction rate. It can use by release film, laminating film and tape because it has excellent run, easy treatment by suitable product. Also, it is a product that thickness control is possible according to customer needs. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面张力 surface tension |
|||
50.0 µm 50.0 µm |
52 | mN/m | |
125.0 µm 125.0 µm |
52 | mN/m | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
摩擦系数 friction coefficient |
|||
与自身 - 动态 With oneself - dynamic |
0.30 | ASTM D1894 | |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
ASTM D882 | ||
MD,屈服,50 µm MD, yield, 50 µ m |
196 | MPa | ASTM D882 |
MD,屈服,75 µm MD, yield, 75 µ m |
196 | MPa | ASTM D882 |
MD,屈服,100 µm MD, yield, 100 µ m |
MPa | ASTM D882 | |
MD,屈服,130 µm MD, yield, 130 µ m |
MPa | ASTM D882 | |
TD,屈服,50 µm TD, yield, 50 µ m |
MPa | ASTM D882 | |
TD,屈服,75 µm TD, yield, 75 µ m |
MPa | ASTM D882 | |
TD,屈服,100 µm TD, yield, 100 µ m |
MPa | ASTM D882 | |
TD,屈服,130 µm TD, yield, 130 µ m |
MPa | ASTM D882 | |
拉伸应变 Tensile strain |
ASTM D882 | ||
MD,断裂,50 µm MD, fracture, 50 µ m |
% | ASTM D882 | |
MD,断裂,75 µm MD, fracture, 75 µ m |
% | ASTM D882 | |
MD,断裂,100 µm MD, fracture, 100 µ m |
% | ASTM D882 | |
MD,断裂,130 µm MD, fracture, 130 µ m |
% | ASTM D882 | |
TD,断裂,50 µm TD, fracture, 50 µ m |
% | ASTM D882 | |
TD,断裂,75 µm TD, fracture, 75 µ m |
% | ASTM D882 | |
TD,断裂,100 µm TD, fracture, 100 µ m |
% | ASTM D882 | |
TD,断裂,130 µm TD, fracture, 130 µ m |
% | ASTM D882 | |
F5 F5 |
ASTM D882 | ||
MD:50.0 µm MD:50.0 µm |
MPa | ASTM D882 | |
MD:75.0 µm MD:75.0 µm |
MPa | ASTM D882 | |
MD:100.0 µm MD:100.0 µm |
MPa | ASTM D882 | |
MD:125.0 µm MD:125.0 µm |
MPa | ASTM D882 | |
TD:50.0 µm TD:50.0 µm |
MPa | ASTM D882 | |
TD:75.0 µm TD:75.0 µm |
MPa | ASTM D882 | |
TD:100.0 µm TD:100.0 µm |
MPa | ASTM D882 | |
TD:125.0 µm TD:125.0 µm |
MPa | ASTM D882 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
ASTM D523 | ||
60°,50.0 µm 60°,50.0 µm |
ASTM D523 | ||
60°,75.0 µm 60°,75.0 µm |
ASTM D523 | ||
60°,100 µm 60°,100 µm |
ASTM D523 | ||
60°,125 µm 60°,125 µm |
ASTM D523 | ||
透光率 Transmittance |
ASTM D1003 | ||
50.0 µm 50.0 µm |
% | ASTM D1003 | |
75.0 µm 75.0 µm |
% | ASTM D1003 | |
100 µm 100 µm |
% | ASTM D1003 | |
125 µm 125 µm |
% | ASTM D1003 | |
雾度 Haze |
ASTM D1003 | ||
50 µm 50 µm |
% | ASTM D1003 | |
75.0 µm 75.0 µm |
% | ASTM D1003 | |
100 µm 100 µm |
% | ASTM D1003 | |
125 µm 125 µm |
% | ASTM D1003 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热收缩 Thermal shrinkage |
内部方法 | ||
MD,30 min:125.0 µm MD,30 min:125.0 µm |
% | 内部方法 | |
MD,30 min:150℃,50.0 µm MD,30 min:150℃,50.0 µm |
% | 内部方法 | |
MD,30 min:150℃,75.0 µm MD,30 min:150℃,75.0 µm |
% | 内部方法 | |
MD,30 min:150℃,100.0 µm MD,30 min:150℃,100.0 µm |
% | 内部方法 | |
TD,30 min:150℃,50.0 µm TD,30 min:150℃,50.0 µm |
% | 内部方法 | |
TD,30 min:150℃,75.0 µm TD,30 min:150℃,75.0 µm |
% | 内部方法 | |
TD,30 min:150℃,100.0 µm TD,30 min:150℃,100.0 µm |
% | 内部方法 | |
TD,30 min:150℃,125.0 µm TD,30 min:150℃,125.0 µm |
% | 内部方法 | |
Surface Treatment Surface Treatment |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
医院供认“塑料为癌症首恶”宣传有误
2016-06-08 最近几天,一张图片刷爆朋友圈。图片上是河南省胸科医院营养科的一则“重要信息”,上写根据美国医生协会的最新研究,发现癌症的起因是塑料。这一消息迅速引发无数网友关注,纷纷转发扩散。但经晚报记者调查发现,所谓的“致癌的起因是塑料”又是一则没有依据的不实信息。 【网曝】“塑料是致癌主因”刷爆朋友圈 这张被四处转发的图片是一张彩色的宣传牌,标题为红色大字“重要信息”,上面写着:“4月21日,美国医生协会已经找到癌病起因的答案:塑料!当 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |