NANCAR® 2845是一种中等耐油性的中丙烯腈-丁二烯共聚物。它在低温下聚合,并含有足够的抗氧化剂,以满足正常老化条件。这是南萨尔2865的低穆尼版本。它具有较低的门尼粘度、优良的加工特性、快速的固化速度、较低的霉菌污染、优良的回弹性能和优越的流动性。NANCAR® 2845建议用于需要改进低温性能的应用中。它提供优秀的挤压和一般的加工改进。 NANCAR® 2845 is a medium acrylonitrile butadiene copolymer with medium oil resistance. It is polymerized at low temperature and contains sufficient antioxidant for normal aging conditions. It is a low Mooney version of NANCAR 2865. It has low Mooney viscosity, superior processing characteristics, fast curing rate, low mold fouling, superior resilience properties and superior flowability. NANCAR® 2845 is recommended for use in applications requiring improved low temperature properties. It provides excellent extrusions and general processing improvement. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.970 | g/cm³ | |
门尼粘度 Mooney viscosity |
|||
ML 1+4,100℃ ML 1+4,100℃ |
46 | MU | ASTM D1646 |
丙烯腈含量(Bound) Acrylonitrile content (Bound) |
28.0 | % | 内部方法 |
Stabilizer Stabilizer |
Non-staining | ||
可溶性 solubility |
|||
in MEK in MEK |
100 | % | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
ASTM D2240 | ||
邵氏 A Shaw's A 2 |
ASTM D2240 | ||
邵氏 A Shaw's A 3 |
ASTM D2240 | ||
邵氏 A Shaw's A 4 |
ASTM D2240 | ||
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
ASTM D412 | ||
300% 应变 300% strain 5 |
MPa | ASTM D412 | |
300% 应变 300% strain 6 |
MPa | ASTM D412 | |
300% 应变 300% strain 7 |
MPa | ASTM D412 | |
拉伸强度 tensile strength |
ASTM D412 | ||
屈服 yield 2 |
MPa | ASTM D412 | |
屈服 yield 3 |
MPa | ASTM D412 | |
屈服 yield 4 |
MPa | ASTM D412 | |
拉伸应变 Tensile strain |
ASTM D412 | ||
断裂 fracture 5 |
% | ASTM D412 | |
断裂 fracture 6 |
% | ASTM D412 | |
断裂 fracture 7 |
% | ASTM D412 | |
撕裂强度 tear strength 8 , 3 |
kN/m | ASTM D624 | |
压缩形变 Compression deformation 4 |
|||
100℃,70 hr 100℃,70 hr 4 |
% | ASTM D395 | |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 The rate of change in tensile strength in air 3 |
|||
100℃,70 hr 100℃,70 hr 3 |
% | ASTM D865 | |
空气中极限伸长率的变化率 The rate of change in ultimate elongation in air 3 |
|||
100℃,70 hr 100℃,70 hr 3 |
% | ASTM D865 | |
空气中硬度计硬度的变化率 The rate of change in hardness of a hardness tester in the air 3 |
|||
邵氏 A,100℃,70 hr Shore A, 100 ℃, 70 hr 3 |
ASTM D865 | ||
拉伸强度的变化率 The rate of change in tensile strength 3 |
ASTM D471 | ||
100℃,70 hr,在ASTM #1油中 100 ℃, 70 hr, in ASTM # 1 oil |
% | ASTM D471 | |
100℃,70 hr,在ASTM #3油中 100 ℃, 70 hr, in ASTM # 3 oil |
% | ASTM D471 | |
极限伸长率的变化率 Change rate of ultimate elongation 3 |
ASTM D471 | ||
100℃,70 hr,在ASTM #1油中 100 ℃, 70 hr, in ASTM # 1 oil |
% | ASTM D471 | |
100℃,70 hr,在ASTM #3油中 100 ℃, 70 hr, in ASTM # 3 oil |
% | ASTM D471 | |
邵氏硬度的变化率 The rate of change in Shore hardness 3 |
ASTM D471 | ||
支撐 A,100℃,70 hr,在ASTM #1油中 Support A, 100 ℃, 70 hr, in ASTM # 1 oil |
ASTM D471 | ||
支撐 A,100℃,70 hr,在ASTM #3油中 Support A, 100 ℃, 70 hr, in ASTM # 3 oil |
ASTM D471 | ||
体积变化 Volume change 3 |
ASTM D471 | ||
100℃,70 hr,ASTM 标准油(1号) 100 ℃, 70 hr, ASTM standard oil (No.1) |
% | ASTM D471 | |
100℃,70 hr,ASTM 标准油(3号) 100 ℃, 70 hr, ASTM standard oil (No.3) |
% | ASTM D471 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热损耗 Heat loss |
% | ASTM D5688 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 硫化 20.0 min 在 302°F |
3 硫化 40.0 min 在 302°F |
4 硫化 60.0 min 在 302°F |
5 Cured for 60.0 min at 150°C |
6 Cured for 40.0 min at 150°C |
7 Cured for 20.0 min at 150°C |
8 C 模具 |
【新闻资讯】查看全部
中德工业4 0技术展现创新中心在苏州停业
2015-12-02 中国―德国工业4.0技术展示创新中心日前于苏州正式开业。此创新中心是一个合作技术平台,可以开展高规格培训,旨在促进中德企业联合研究和工业4.0创新项目的建立实施,促进两国先进技术共享,推动工业4.0在中国的发展,同时培养人才。 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |