牌号简介 About |
---|
Visico™ LE4423/LE4437是一种用于低压绝缘的防焦、湿交联聚乙烯化合物。 Visico LE4423/LE4437 is a scorch retardant, moisture-crosslinking polyethylene compound for low voltage insulation The combination of a VISICO base material, LE4423, and a tin catalyst masterbatch, LE4437, provides a highly scorch retardant compound with excellent thermal stability. LE4423/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. LE4437 should be added to LE4423 directly in the extruder hopper by dry blending a ratio of 5 parts LE4437 to 95 parts LE4423. LE4437 also provides, in addition to catalyst, a stabilizaton package containing suitable antioxidants, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, LE4423/LE4437 exhibits excellent thermal stability to oxidation. LE4423/LE4437 is readily pigmented to a variety of colors using standard wire & cable concentrates designed for thermoplastic or crosslinked polyethylene. UV weather resistance is obtained by the addition of a suitable carbon black or UV additive. Using VISICO LE4432 in place of LE4437 combines a tin catalyst along with the proper carbon black to provide a black, UV resistant, moisture crosslinking cable insulation. Specifications Visico LE4423/LE4437 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure: Underwriters Laboratories Standards 854 for types USE and USE-2 EC 502 NBN C 33-321 Canadian Standards Association C22.2 No. 1790-00-Airport Series Lighting Cables and C22.2 No. 38 Cable Type RW-90 NF C33-210 HD 603 S1 NF C32-090 ASTM D 2655 Contact your Borealis representative for additional information. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
ASTM D792 | ||
-- -- 2 |
0.923 | g/cm³ | ASTM D792 |
-- -- 3 |
0.941 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate 2 |
0.90 | g/10min | ASTM D1238 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服 yield |
15.0 | MPa | ASTM D412 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
300 | % | ASTM D412 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热固性 thermosetting |
ICEA T-28-562 | ||
150℃ 150℃ 4 |
% | ICEA T-28-562 | |
150℃ 150℃ 5 |
% | ICEA T-28-562 | |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸性能的保留率 Retention rate of tensile performance |
|||
After Ageing 168 h,121℃ After Ageing 168 h,121℃ |
% | IEC 60811-1-2 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
介电强度 Dielectric strength |
kV/mm | ASTM D149 | |
介电常数 Dielectric constant |
|||
23 ℃,60 Hz 23 ℃,60 Hz |
ASTM D150 | ||
耗散因数 Dissipation factor |
|||
23℃,60 Hz 23℃,60 Hz |
ASTM D150 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 LE4423 |
3 LE4437 |
4 Elongation under load, 0.20 MPa |
5 Permanent deformation, 0.20 MPa |
【新闻资讯】查看全部
【干货】注塑拉伸模的常见缺陷,你知道多少?
2021-01-08 搜料网资讯: 1.壁破裂 这种缺陷一般出现在方筒角部附近的侧壁,通常,出现在凹模圆角半径(rcd)附近。在模具设计阶段,一般难以预料。即倒W字形,在其上方出现与拉深方向呈45的交 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |