CALIBRE™ 5101 聚碳酸酯树脂中添加了10%的玻璃纤维增强材料,具有更高的模量,耐热性能更好,收缩减低至最低水平。这种树脂具有优秀的UL94阻燃等级,含有脱模剂。CALIBRE 5101可提供的熔流率有8 和 15 两种。CALIBRE 5101 树脂已经根据ISO 10993 (医疗器械生物学评价)经过了生物相容性测试,适合用于获准的医疗应用领域。 主要特性: 玻璃纤维增强 阻燃 ISO 10993 应用领域 信息技术设备 电信 医疗应用领域 CALIBRE™ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL94 flammability ratings and contains mold release. CALIBRE 5101 is available in 8 and 15 melt flow rates. CALIBRE 5101 resin has undergone biocompatibility testing based on ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications. Main Characteristics: Glass reinforced Ignition resistant Tested under ISO 10993 Applications Information Technology Equipment Telecommunications Medical applications |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.27 | g/cm³ | ASTM D792 |
密度 Density |
1.27 | g/cm³ | ISO 1183/B |
密度 Density |
1.27 | g/cm³ | ISO 1183-3 |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,1.20kg 300℃,1.20kg |
15 | g/10min | ASTM D1238 |
300℃,1.20kg 300℃,1.20kg |
15 | g/10min | ISO 1133 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,1.2 kg 300℃,1.2 kg |
cm³/10min | ISO 1133 | |
收缩率 Shrinkage rate |
|||
MD MD |
% | ISO 294-4 | |
MD MD |
% | ASTM D955 | |
吸水率 Water absorption rate |
|||
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ASTM D570 | |
23℃,24hr 23℃,24hr |
% | ASTM D570 | |
23℃,24hr 23℃,24hr |
% | ISO 62 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁冲击强度 Charpy impact strength |
|||
23℃ 23℃ |
ISO 179/1eU 3 | ||
-30℃ -30℃ |
ISO 179/1eU 3 | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃ 23℃ |
J/m | ASTM D256 | |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments 7 |
|||
23℃,Total Energy 23℃,Total Energy 7 |
J | ASTM D3763 | |
拉伸冲击强度 Tensile impact strength |
kJ/m² | ASTM D1822 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
1.8 MPa 1.8 MPa |
℃ | ISO 75-2 3 | |
0.45 MPa,退火 0.45 MPa, annealed |
℃ | ISO 75-2/B | |
0.45 MPa,退火 0.45 MPa, annealed |
℃ | ASTM D648 | |
0.45 MPa 0.45 MPa |
℃ | ISO 75-2 3 | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 8 | |
B50 B50 |
℃ | ISO 306 | |
B50 B50 |
℃ | ISO 306 3 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:-40~82℃ MD:-40~82℃ |
1/℃ | ASTM D696 | |
MD MD |
1/℃ | ISO 11359-2 3 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level 9 |
UL 94 | ||
1.60 mm 1.60 mm |
UL 94 | ||
3.20 mm 3.20 mm |
UL 94 | ||
阻燃等级 Flame retardant level |
|||
3.20 mm 3.20 mm |
ISO 1210 3 | ||
极限氧指数 Extreme oxygen index 9 |
% | ISO 4589-2 | |
氧指数 Oxygen index |
% | ISO 4589-2 3 | |
平均燃烧程度 Average combustion degree |
cm | ASTM D635 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 4 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-2/50 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-2 3 | |
拉伸强度 tensile strength 4 |
|||
断裂 fracture |
MPa | ISO 527-2/50 | |
断裂 fracture 4 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
屈服 yield |
MPa | ISO 527-2 3 | |
屈服 yield 4 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
屈服 yield |
% | ISO 527-2 3 | |
Nominal strain at break Nominal strain at break |
% | ISO 527-2 3 | |
弯曲模量 Bending modulus 5 |
MPa | ASTM D790 | |
弯曲模量 Bending modulus 6 |
MPa | ISO 178 | |
弯曲强度 bending strength 5 |
MPa | ASTM D790 | |
弯曲强度 bending strength 6 |
MPa | ISO 178 | |
洛氏硬度 Rockwell hardness |
ASTM D785 | ||
M 级 M-level |
ASTM D785 | ||
R 级 R-level |
ASTM D785 | ||
特殊值 |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
1.60 mm 1.60 mm |
ISO 1210 3 |
备注 |
---|
1 Biocompatibility testing following ISO Guidelines 10993 has been completed on select classic resins in this series. Please consult Styron for details. ISO guidelines include a sensitization test. |
2 一般属性:这些不能被视为规格。 |
3 ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
4 2.0 in/min |
5 方法 I (三点负荷), 0.079 in/min |
6 0.079 in/min |
7 11.1 ft/sec |
8 速率 A (50°C/h), 载荷2 (50N) |
9 这个额定值并非为了反映这种或任何其他材料在实际起火条件下造成的危险。 |
10 This rating not intended to reflect hazards presented by this or any other material under actual fire conditions. |
【新闻资讯】查看全部
帝斯曼推出帝安瑞TM水性植物基高功用涂料树脂
2018-12-03 专注于营养、健康和绿色生活的全球科学公司荷兰皇家帝斯曼集团宣布面向中国市场推出帝安瑞TM(Decovery®)环保涂料解决方案。该水性植物基树脂技术平台集高性能和可持续性优势于一体,代表了帝斯曼所取得的一项革命性技术突破:利用可再生原料取代化石原料,以满足市场对环保型建筑及家具日益增长的需求。 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |