K50-10-136是一种高分子量、高密度聚乙烯共聚物,用于吹塑汽车油箱和发动机罩下油箱。它结合了优良的加工性能和优异的物理性能,特别是环境应力抗裂性(ESCR)和冲击性能。 K50-10-136 is a high molecular weight, high density polyethylene copolymer for blow molding automotive fuel tanks and under hood reservoirs. It combines excellent processability and outstanding physical performance, particularly environmental stress crack resistance (ESCR) and impact properties. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.950 | g/cm³ | ASTM D4883 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,21.6kg 190℃,21.6kg |
9.0 | g/10min | ASTM D1238 |
抗环境应力开裂 ESCR(Environmental Stress Cracking Resistance) |
|||
10%非离子洗涤剂,F50 10% non-ionic detergent, F50 |
430 | hr | ASTM D1693A |
10%非离子洗涤剂,F50 10% non-ionic detergent, F50 |
340 | hr | ASTM D1693B |
100%非离子洗涤剂,F50 100% non-ionic detergent, F50 |
> 1000 | hr | ASTM D1693A |
100%非离子洗涤剂,F50 100% non-ionic detergent, F50 |
hr | ASTM D1693B | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 D Shaw's D |
ASTM D2240 | ||
拉伸强度 tensile strength 2 |
|||
断裂 fracture 2 |
MPa | ASTM D638 | |
屈服 yield 2 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain 2 |
|||
断裂 fracture 2 |
% | ASTM D638 | |
屈服 yield 2 |
% | ASTM D638 | |
弯曲模量 Bending modulus |
ASTM D790A | ||
2% 正割 2% secant |
MPa | ASTM D790-A | |
正切 tangent |
MPa | ASTM D790-A | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
J/m | ASTM D256 | |
Area Area |
kJ/m² | ASTM D256 | |
Instrumented Impact,Ductility Instrumented Impact,Ductility |
ASTM D3763 | ||
-30℃ -30℃ |
ASTM D3763 | ||
23℃ 23℃ |
ASTM D3763 | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ASTM D648 | |
脆化温度 Embrittlement temperature |
℃ | ASTM D746 | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
【新闻资讯】查看全部
【干货】注塑成型工艺对产品性能有何影响?
2021-03-08 搜料网资讯: 传统的模具设计和工艺参数设置主要依赖于设计者的经验和技巧,模具设计的合理性只有靠反复的试模和修模,工艺参数的设置也只能靠反复的试模来进行修改,缺乏科学依据 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |