产品描述:三丁橡胶A64NU是一种热稳定的PP/EPDM基热塑性硫化弹性体(TPV)。这种天然化合物主要用于发动机罩下的应用,如垫子、密封件、垫圈、风管、CVJ护套、盖子、索环或其他需要柔软性和一致性的零件。这种材料可以使用注塑、挤压、吹塑或其他熔融加工技术进行加工。 Product Description: TREXPRENE ® A64NU is a heat stabilized PP/EPDM based Thermoplastic Vulcanized Elastomer (TPV). This Natural compound is intended primarily for underhood applications such as mats, seals, gaskets, air ducts, CVJ boots, covers, grommets or other parts where softness and conformity are needed. This material can be processed using Injection Molding, Extrusion, Blow Molding or other melt processing techniques. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.930 to 0.970 | g/cm³ | ISO 1183 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength 2 |
ISO 37 | ||
TD,100% 应变 TD, 100% strain |
2.30 | MPa | ISO 37 |
MD,100% 应变 MD, 100% strain |
3.90 | MPa | ISO 37 |
拉伸强度 tensile strength 2 |
ISO 37 | ||
断裂 fracture |
5.70 | MPa | ISO 37 |
MD,断裂 MD, fracture |
4.50 | MPa | ISO 37 |
拉伸应变 Tensile strain 2 |
ISO 37 | ||
断裂 fracture |
% | ISO 37 | |
流量,断裂 Flow rate, fracture |
% | ISO 37 | |
撕裂强度 tear strength 3 |
ISO 34-1 | ||
TD TD |
kN/m | ISO 34-1 | |
MD MD |
kN/m | ISO 34-1 | |
压缩形变 Compression deformation |
ASTM D395B | ||
70℃,22 hr 70℃,22 hr |
% | ASTM D395B | |
125℃,70 hr 125℃,70 hr |
% | ASTM D395B | |
压缩形变 Compression deformation 4 |
ISO 815 | ||
70℃,22 hr 70℃,22 hr |
% | ISO 815 | |
125℃,70 hr 125℃,70 hr |
% | ISO 815 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,15 秒 Shore A, 15 seconds |
ISO 868 | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Embrittlement temperature |
℃ | ASTM D746 | |
Brittleness Temperature(Type B) Brittleness Temperature(Type B) |
℃ | ISO 812 | |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 The rate of change in tensile strength in air |
ISO 188 | ||
110℃,1000 hr 110℃,1000 hr |
% | ISO 188 | |
150℃,168 hr 150℃,168 hr |
% | ISO 188 | |
在空气中断裂时拉伸应力变化 Changes in tensile stress during fracture in air |
ISO 188 | ||
110℃,1000 hr 110℃,1000 hr |
% | ISO 188 | |
150℃,168 hr 150℃,168 hr |
% | ISO 188 | |
Change in Tensile Stress(125℃,70 hr,in IRM 903 Oil) Change in Tensile Stress(125℃,70 hr,in IRM 903 Oil) |
% | ISO 1817 | |
Change in Tensile Strain at Break(125℃,70 hr,in IRM 903 Oil) Change in Tensile Strain at Break(125℃,70 hr,in IRM 903 Oil) |
% | ISO 1817 | |
体积变化 Volume change |
|||
125℃,70 hr,在IRM 903油中 125 ℃, 70 hr, in IRM 903 oil |
% | ISO 1817 | |
撕裂强度的变化率 Change rate of tear strength |
|||
70 hrs,in IRM 903 Oil,125℃ 70 hrs,in IRM 903 Oil,125℃ |
% | ISO 1817 | |
Change in Tensile Properties Change in Tensile Properties |
|||
Stress at 100% Elongation in Air,168 hrs:150℃ Stress at 100% Elongation in Air,168 hrs:150℃ |
% | ISO 188 | |
Stress at 100% Elongation in IRM 903 Oil,70 hrs:125℃ Stress at 100% Elongation in IRM 903 Oil,70 hrs:125℃ |
% | ISO 1817 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
燃烧速率 Burning rate |
mm/min | ISO 3795 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
耐臭氧性 Ozone resistance 5 |
|||
40℃ 40℃ 5 |
ISO 1431-1 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 类型 1, 20 in/min |
3 B 方法,直角形试样(不割口), 20 in/min |
4 类型 A |
5 100 pphm, Method A |
【新闻资讯】查看全部
新资料:构造性过剩与核心技术缺失难题待解
2017-03-08 专家建议,通过“政策性引导+市场化环境”,推动产业发展“规模效应” 材料科学是战略性新兴产业的基础科学,对我国实施创新驱动发展战略至关重要。但目前,我国这一领域的竞争力堪忧,一方面核心关键材料对外依存度较高,关键技术缺失;另一方面,有些项目却“一哄而上”,出现产业结构性过剩。有人直言“急需的新材料找不到、能找到的又做不出、做得出的又做不好”。 目前,深圳等一些地方已通过“政策性引导+市场化环境”形成“磁吸效应”,吸引全球顶尖新材料创新人才前来创业。一些专家建 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |