公司信息及水印
牌号简介 About |
---|
Promyde® B30 P2 G30是一个聚酰胺6 UL认证的注塑等级,30%的玻璃纤维和热稳定。特点Promyde® B30 P2 G30具有高机械强度、硬度、刚度、热稳定性(熔点220°C)和耐高温润滑剂和水性。由Promyde® B30 P2 G30制成的零件具有特别高的尺寸稳定性和蠕变强度。应用Promyde® B30 P2 G30广泛应用于需要机械性能和热阻组合的各种应用中。玻璃纤维增强等级适用于外壳、支架、工业品和电气绝缘部件。 Promyde B30 P2 G30 is a Polyamide 6 UL certified injection moulding grade with 30% glass fibre and heat stabilized. CHARACTERISTICS Promyde B30 P2 G30 is distinguished by high mechanical strength, hardness, rigidity, thermo stability (melting point 220°C), and resistance to hot lubricants and water. Parts made from Promyde B30 P2 G30 have particularly high dimensional stability and creep strength. APPLICATIONS Promyde B30 P2 G30 is used in a wide range of applications where a combination of mechanical properties and thermal resistance is needed. Glass-fibre reinforced grades are suitable for housings, supports, industrial articles and electrical insulating parts. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.36 | g/cm³ | ISO 1183 |
熔体体积流动速率 Melt Volume Rate |
|||
275℃,5 kg 275℃,5 kg |
45.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
TD TD |
0.40 to 0.45 | % | |
MD MD |
0.30 to 0.35 | % | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
6.7 | % | ISO 62 |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
粘数 Viscosity number |
cm³/g | ISO 307 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2/50 | |
标称拉伸断裂应变 Nominal tensile fracture strain |
|||
23℃ 23℃ |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus |
|||
23℃ 23℃ |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
23℃ 23℃ |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eU | |
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | ISO 3146 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:23~80℃ TD:23~80℃ |
1/℃ | ISO 11359-2 | |
MD:23~80℃ MD:23~80℃ |
1/℃ | ISO 11359-2 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电常数 Dielectric constant |
|||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
|||
1 MHz 1 MHz |
IEC 60250 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
1.50 mm 1.50 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 0.079 in/min |
3 10°C/min |
【新闻资讯】查看全部
新型PC/PBT共混物具有高冲击强度,可减少翘曲倾向和提高紫外线稳定性
2020-10-19 搜料网资讯: 德国Romira开发了一种PC/PBT共混物,具有特别高的冲击强度,可减少翘曲倾向和提高紫外线稳定性。Romiloy EXP3008在抗紫外线方面表现出非常好的性能。 PC/PBT混合物是结合了无 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |