牌号简介 About |
---|
PA 66注射成型,化学增强20%玻璃纤维,热稳定,适用于高强度和高冲击成型。用于汽车、工程和电气行业。可用于长期热冲击高达200°C的环境中。在170°C下5000小时后,拉伸强度降低50%。热稳定性预先确定了产品对长期热暴露环境的影响,如进气管、气缸盖、感应线圈、电机区域内固定的电机承载部件。应用:汽车工业中的爱好工具、齿轮、电动工具盖、冷却水分配。以黑色交付。 PA 66 for injection moulding, chemically reinforced with 20 % glass fibre, heat stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and electrical industry. Can be used in environment, in which longtime heat impact of up to 200°C occurs. Decrease in tensile strength by 50 % after 5000 hours at 170°C. The heat stabilization predetermines the products to environment with longtime heat exposure, like eg. intake pipes, cylinder heads, induction coils, carrying parts in the motor fixing in the motor area. Application: hobby tools, gears, covers of electric tools, cooling water distribution in the automotive industry. Delivered in black. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.29 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
275℃,0.325kg 275℃,0.325kg |
3.0 | g/10min | ISO 1133 |
收缩率 Shrinkage rate |
STM 64 0808 | ||
TD TD |
1.1 | % | STM 64 0808 |
MD MD |
0.36 | % | STM 64 0808 |
含水量 water content |
0.15 | % | ISO 960 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
MPa | ISO 527-2 | |
拉伸强度 tensile strength |
|||
屈服 yield |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
|||
屈服 yield |
% | ISO 527-2 | |
弯曲模量 Bending modulus |
MPa | ISO 178 | |
弯曲强度 bending strength |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179 | ||
-20℃ -20℃ |
kJ/m² | ISO 179 | |
23℃ 23℃ |
kJ/m² | ISO 179 | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179 | ||
-20℃ -20℃ |
kJ/m² | ISO 179 | |
23℃ 23℃ |
kJ/m² | ISO 179 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
维卡软化温度 Vicat Softening Temp |
℃ | ISO 306/B | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | ISO 3146 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
kV/mm | IEC 60243-1 | |
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
灼热丝起燃温度 Igniting temperature of the hot wire |
℃ | IEC 60695-2-13 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
Teknor Apex推出新的尼龙化合物 用于汽车和电子产品
2021-05-09 搜料网资讯: 近日,位于R.I. Pawtucket的Teknor Apex公司高管在一份新闻稿中说,这些新的Creamid品牌材料不含卤素,具有阻燃性和玻璃强化功能。与标准的玻璃填充的阻燃尼龙66相比,这些化 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |