公司信息及水印
牌号简介 About |
---|
Amodel HFZ A- 4133 L聚邻苯二甲酰胺(PPA)是一种33%玻纤维增强、热水可成形树脂。主要性能包括耐热性、在宽的温度范围内降低了气体排放、高强度和刚度、低吸湿性、优异的耐化学性和优良的电性能。 Amodel HFZ A- 4133 L树脂是汽车电气、电子产品,包括连接器、插座、开关和传感器等的理想选择。也是发动机罩下用于保护关键控制系统,如防抱死制动系统、牵引力控制系统、转向系统、发动机电子控制、传动和底盘控制单元等外壳的不错选择。 - 黑色:HFZ A-4133 L BK 324 本色: HFZ A-4133 L NT Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad temperature range. It also displays low moisture absorption, excellent chemical resistance and excellent electrical properties. Amodel® HFZ A-4133 L resin is ideal for automotive electrical and electronic applications, including connectors, sockets, switches and sensors. It is also a good choice for under-hood enclosures that protect critical control systems such as anti-lock brakes, traction control, steering, electronic engine control, transmission and chassis control units. Black: HFZ A-4133 L BK 324 Natural: HFZ A-4133 L NT |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.46 | g/cm³ | ISO 1183/A |
收缩率 Shrinkage rate |
|||
TD TD |
1.0 | % | ASTM D955 |
MD MD |
0.50 | % | ASTM D955 |
吸水率 Water absorption rate |
|||
24hr 24hr |
0.26 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
12000 | MPa | ISO 527-2 |
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2 | |
弯曲模量 Bending modulus |
MPa | ISO 178 | |
弯曲强度 bending strength |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
kJ/m² | ISO 179-1eA | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
kJ/m² | ISO 180/1U | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | ISO 3146 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD TD |
ASTM E831 | ||
0 到 90℃ 0 to 90 ℃ |
cm/cm/℃ | ASTM E831 | |
150 到 250℃ 150 to 250 ℃ |
cm/cm/℃ | ASTM E831 | |
MD MD |
ASTM E831 | ||
0 到 90℃ 0 to 90 ℃ |
cm/cm/℃ | ASTM E831 | |
150 到 250℃ 150 to 250 ℃ |
cm/cm/℃ | ASTM E831 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | ASTM D257 | |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
介电强度 Dielectric strength |
kV/mm | ASTM D149 | |
介电常数 Dielectric constant |
ASTM D150 | ||
60 Hz 60 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
耗散因数 Dissipation factor |
ASTM D150 | ||
60 Hz 60 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
高压电弧抗点燃指数(HVAR)(PLC) High voltage arc ignition resistance index (HVAR) (PLC) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
0.80 mm 0.80 mm 2 |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
℃ | IEC 60695-2-13 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 这些可燃性等级不代表这些材料或任何其他材料在实际着火灾情况下的危险性。 |
【新闻资讯】查看全部
一宗化工行业并购交易在美国宣告诞生
2021-04-10 搜料网资讯: 全球化工行业并购活动势头强劲,一宗新的交易在美国宣告诞生。当地时间3月20日,美国涂料巨头宣伟Sherwin-Williams)宣布,将斥资113亿美元收购同行威士伯(Valspar)。 根据协 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |