Solef ® 60512 PVDF共聚物熔体粘度高,是离岸管道级材料。 Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.75 to 1.80 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,10.0kg 230℃,10.0kg |
2.5 to 4.0 | g/10min | ASTM D1238 |
收缩率 Shrinkage rate |
|||
MD MD |
2.0 to 3.0 | % | |
吸水率 Water absorption rate |
|||
23℃,24hr 23℃,24hr |
< 0.040 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 D,2.00 mm Shore D, 2.00 mm |
70 | ASTM D2240 | |
拉伸模量 Tensile modulus 2 |
|||
23℃,2 mm 23℃,2 mm 2 |
MPa | ASTM D638 | |
拉伸强度 tensile strength 3 |
|||
断裂,23℃,2 mm Fracture, 23 ℃, 2 mm 3 |
MPa | ASTM D638 | |
屈服,23℃,2 mm Yield, 23 ℃, 2 mm 3 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain 3 |
|||
断裂,23℃,2 mm Fracture, 23 ℃, 2 mm 3 |
% | ASTM D638 | |
屈服,23℃,2 mm Yield, 23 ℃, 2 mm 3 |
% | ASTM D638 | |
摩擦系数 friction coefficient |
ASTM D1894 | ||
与自身 - 动态 With oneself - dynamic |
ASTM D1894 | ||
与自身 - 静态 With oneself - static |
ASTM D1894 | ||
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,CS-10 转轮 1000 cycles, 1000 g, CS-10 wheels |
mg | ASTM D4060 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 4 |
|||
23℃,4mm 23℃,4mm 4 |
J/m | ASTM D6110 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
玻璃化转变温度 Glass transition temperature |
℃ | ASTM D4065 | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 5 | |
熔融温度 Melting temperature |
℃ | ASTM D3418 | |
结晶峰温度 Crystallization peak temperature 12 |
|||
DSC DSC 12 |
℃ | ASTM D3418 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:0~40℃ MD:0~40℃ |
1/℃ | ASTM D696 | |
比热 specific heat |
ASTM E968 | ||
23℃ 23℃ |
J/kg/℃ | ASTM E968 | |
100℃ 100℃ |
J/kg/℃ | ASTM E968 | |
导热系数 Thermal conductivity coefficient |
|||
23℃ 23℃ |
W/m/K | ASTM C177 | |
结晶热 Crystallization heat |
J/g | ASTM D3417 | |
融合热量 Fusion heat |
J/g | ASTM D3417 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | ASTM D257 | |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 类型 4, 0.039 in/min |
3 类型 4, 2.0 in/min |
4 2 m/s,部分断裂 |
5 速率 A (50°C/h), 载荷2 (50N) |
【新闻资讯】查看全部
山西省委书记林武到潞安化工集团调研
2022-02-19 二月十五日,山西省委书记林武来到山西潞安煤基清洁能源公司,听取180万吨/年高硫煤清洁利用油化电热一体化项目脱困措施和提质增效情况汇报。史晓波/摄 2月14日至15日,山西省委 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |